Chemical Composition and Analysis

All analyses were conducted following Indian Standards (IS) and international testing protocols. The results are summarized below:

Parameter Result (%) Industrial Significance
Silica (SiO₂) 80.02% Provides thermal insulation and dielectric properties.
Alumina (Al₂O₃) 13.05% Enhances thermal resistance and dielectric strength.
Ferric Oxide (Fe₂O₃) 0.46% Contributes to mechanical strength with mild coloration.
Titania (TiO₂) Nil Improves color consistency and transparency.
Lime (CaO) 0.19% Acts as flux in ceramic processing.
Magnesia (MgO) 0.24% Improves thermal shock resistance.
Soda (Na₂O) 4.03% Reduces fusion temperature in glass formulations.
Potash (K₂O) 0.96% Improves dielectric and insulation performance.
Loss on Ignition 0.74% Indicates minor volatile presence from mica minerals.